MODEL

ACM-1B Blade

INTRO

ACM-1B Blade
Main Performance
It is made of 40% carbon fiber, 60% high-strength glass fiber, high-temperature resin adhesive and high-performance wear-resistant lubricating materials.
The operating temperature shall be equal to or lower than 200℃. The blade offers good wear resistance, without any damage to roller and high cleaning efficiency, thus making it applicable to the ceramic roller in the press section, hard rubber roller, hard resin roller and chromed roller.

It is made of 40% carbon fiber, 60% high-strength glass fiber, high-temperature resin adhesive and high-performance wear-resistant lubricating materials.
The operating temperature shall be equal to or lower than 200℃. The blade offers good wear resistance, without any damage to roller and high cleaning efficiency, thus making it applicable to the ceramic roller in the press section, hard rubber roller, hard resin roller and chromed roller.